• VT-42S Laminate/Prepreg

    UL Approval: E214381 Version: B5 28/12/2017 /21/24

    General Information

    • Dicy Cured System
    • Standard FR4.0 (Tg150℃)
    • UV Blocking

     

    Application

    Computer, Communication Equipment, Instrumentation, TV, VCR, Electronic Game Machine, LCD, Automotive, etc

    Availability

    • Core Thickness: 0.002” (0.05mm) to 0.200” (5mm), available in sheet or panel form
    • Copper Foil: 1/4oz to 12oz
    • Prepregs are available in roll or panel form
    • E-Glass styles: 7628, 1506, 1500, 2113, 2313, 3313, 2116, 1080, 1086, 1078, 106 & 1067, etc.

     

    Properties Prepreg Laminate
    Storage Condition Temperature Below 23°C (73°F) Below 5°C (41°F) Room
    Relative humidity Below 55% RH / /
    Shelf Life 3 months 6 months 24 months (airproof)

    The prepreg exceeding shelf life should be retested.

    Properties Sheets IPC-4101E /24 (most compliant), /21

    Properties Test Method Units Specification Typical Value
    Thermal Properties
    Tg DSC IPC-TM-650 2.4.25 °C 145 minimum 150
    TMA IPC-TM-650 2.4.24 °C - -
    Td ASTM D3850 °C - 315
    T260 IPC-TM-650 2.4.24.1 Minute - 25
    T288 IPC-TM-650 2.4.24.1 Minute - 2
    Thermal Stress @ 288°C IPC-TM-650 2.4.13.1 Second Pass 10s 300
    Z-axis CTE Before Tg IPC-TM-650 2.4.24 ppm/°C - 50
    After Tg IPC-TM-650 2.4.24 ppm/°C - 250
    Total Expansion (50~260°C) IPC-TM-650 2.4.24 % - 3.75
    X-Y CTE IPC-TM-650 2.4.24 ppm/°C - 12~14
    MOT UL 94 °C - 130
    Electrical Properties
    DK @ 1GHz RC 50% IPC-TM-650 2.5.5.9 - 5.4 maximum 4.2
    DF @ 1GHz RC 50% IPC-TM-650 2.5.5.9 - 0.035 maximum 0.015
    Volume Resistivity After Moisture Resistance IPC-TM-650 2.4.17.1 MΩ-cm 1.0E+6 minimum 5.0E+8
    E-24/125 IPC-TM-650 2.4.17.1 MΩ-cm 1.0E+3 minimum 5.0E+6
    Surface Resistivity After Moisture Resistance IPC-TM-650 2.4.17.1 1.0E+4 minimum 5.0E+7
    E-24/125 IPC-TM-650 2.4.17.1 1.0E+3 minimum 5.0E+6
    Electrical Strength IPC-TM-650 2.5.6.2 Volt/mil (KV/mm) 762 (30) minimum 1200~1400 (54)
    Dielectric Breakdown IPC-TM-650 2.5.6 KV 40 minimum 60
    Comparative Tracking Index (CTI) ASTM D3638 Rating (Volt) - Grade 3 (175~250)
    Arc Resistance ASTM D495 Second - 240
    Mechanical Properties
    Peel Strength (1oz) As received IPC-TM-650 2.4.8 lb/in (N/mm) - 10~12 (1.7~2.0)
    After thermal stress IPC-TM-650 2.4.8 lb/in (N/mm) 6 (1.05) minimum 9~12 (1.5~2.0)
    Flexural Strength Warp IPC-TM-650 2.4.4 KPsi (MPa) 60 (415) minimum 87 (600)
    Fill IPC-TM-650 2.4.4 KPsi (MPa) 50 (345) minimum 72 (500)
    Physical Properties
    Moisture Absorption IPC-TM-650 2.6.2.1 % 0.8 maximum 0.2
    Flammability UL-94 Rating V-0 minimum V-0

    All test data provided are typical values and not intended to be specification values.

    Published on: 28/12/2017

    Download TDS Datasheet
  • VT-42S CCL/Laminate VT-42S PP/Prepreg (Standard FR4 Material)

    UL Approval: E214381 Version: Rev. B4 27/04/2017 /21/24

    Storage Condition & Shelf Life

    Precautions In Handling

    • The prepreg exceeding shelf time should be retested.
    • Take care in handling thin core laminates as they are easily damaged.
    • If the prepreg is not consumed within 48hrs after opening the vacuum package, it is recommended that the bags be resealed.
    • Material is available in both long and short grain. The grain direction is indicated on the label with an arrow.

     

    Designing And Inner Layer Process

    • Please be careful when single ply of 1080, 1086, 1078 or 106 prepreg is designed to the dielectric layer.
    • Dimension stability is the same as Standard FR4 material.
    • Please check with your oxide vendor to make sure that our material is suitable with your oxide process. We recommend to control the peel strength with brown oxide copper over 2 Lb/in.
    • For unclad or single sided laminates to be used in multilayer, please brush unclad sides before use.

     

    Prepreg Availability

    E-Glass styles: 7628, 1506, 1500, 2113, 2313, 3313, 2116, 1080, 1086, 1078, 106, 1067 etc.

    Prepreg Availability

    PP Type Resin Content Press Thickness (mil) DK DF Remark
    @ 1GHz @ 2GHz @ 5GHz @ 10GHz @ 1GHz @ 2GHz @ 5GHz @ 10GHz
    7628 46% 8.00 4.16 4.11 4.11 4.06 0.014 0.014 0.014 0.016 Standard
    7628 43% 7.60 4.26 4.20 4.20 4.15 0.013 0.013 0.013 0.015 Standard
    1506 52% 7.40 3.98 3.92 3.90 3.85 0.015 0.015 0.016 0.017 Standard
    2116 57% 5.50 3.87 3.82 3.82 3.77 0.016 0.016 0.017 0.018 Standard
    2116 53% 4.90 3.98 3.92 3.90 3.85 0.015 0.015 0.016 0.017 Standard
    2116 50% 4.50 4.05 4.00 4.00 3.95 0.015 0.015 0.016 0.017 Standard
    2113 56% 4.00 3.87 3.82 3.82 3.77 0.015 0.015 0.016 0.017 Standard
    1086 63% 3.40 3.73 3.69 3.65 3.60 0.017 0.017 0.018 0.019 Standard
    1080 68% 3.50 3.63 3.58 3.58 3.53 0.017 0.017 0.018 0.019 Standard
    1080 65% 3.20 3.68 3.63 3.63 3.58 0.017 0.017 0.018 0.019 Standard
    1080 63% 3.00 3.73 3.69 3.65 3.60 0.017 0.017 0.018 0.019 Standard
    1078 65% 3.30 3.68 3.63 3.63 3.58 0.017 0.017 0.018 0.019 Standard
    106 75% 2.50 3.45 3.40 3.40 3.35 0.018 0.018 0.019 0.020 Standard

    ① Press thickness test condition---Prepreg lamination size 18”*24”, Copper Foil---1oz/1oz, Flow---about 5%; ② Make laminated pre-preg to micro-section and measure the thickness with microscope; this thickness is used for resistance design calculation. ③ The thickness measured with micrometer is 0.2~0.4 mil larger than that measured with micro-section; and mainly used for total thickness design calculation.

    Laminate Availablity

    Thickness: 0.002” (0.05mm) to 0.200” (5mm), available in sheet or panel form Copper Foil: 1/4 to 12oz, HTE or RTF or DST DK values are for impedance design.

    Laminate Availability

    Core thk. (Inches) Stack-up Resin Content DK DF Remark
    @ 1GHz @ 2GHz @ 5GHz @ 10GHz @ 1GHz @ 2GHz @ 5GHz @ 10GHz
    0.002 1-106 70% 3.55 3.50 3.50 3.45 0.018 0.018 0.019 0.020 Standard
    0.003 1-1080 63% 3.73 3.69 3.65 3.60 0.017 0.017 0.018 0.019 Standard
    0.004 1-2116 44% 4.17 4.13 4.13 4.08 0.014 0.014 0.015 0.016 Standard
    0.004 2-106 70% 3.55 3.50 3.50 3.45 0.018 0.018 0.019 0.020 2ply
    0.005 1-2116 53% 3.98 3.92 3.90 3.85 0.015 0.015 0.016 0.017 Standard
    0.006 1-1506 45% 4.16 4.11 4.11 4.06 0.014 0.014 0.014 0.016 Standard
    0.007 1-7628 41% 4.27 4.23 4.23 4.18 0.013 0.013 0.013 0.015 Standard
    0.008 1-7628 45% 4.16 4.11 4.11 4.06 0.014 0.014 0.014 0.016 Standard
    0.008 2-2116 44% 4.17 4.13 4.13 4.08 0.014 0.014 0.015 0.016 2ply
    0.010 2-2116 53% 3.98 3.92 3.90 3.85 0.015 0.015 0.016 0.017 Standard
    0.012 2-1506 44% 4.17 4.13 4.13 4.08 0.014 0.014 0.014 0.016 Standard
    0.014 2-7628 40% 4.29 4.25 4.25 4.20 0.013 0.013 0.013 0.015 Standard
    0.016 2-7628 45% 4.16 4.11 4.11 4.06 0.014 0.014 0.014 0.016 Standard
    0.028 4-7628 40% 4.29 4.25 4.25 4.20 0.013 0.013 0.013 0.015 Standard
    0.036 5-7628 42% 4.26 4.20 4.20 4.15 0.013 0.013 0.013 0.015 Standard
    0.045 6-7628 42% 4.35 4.30 4.22 4.22 0.013 0.013 0.013 0.015 Standard
    0.049 7-7628 40% 4.26 4.20 4.20 4.15 0.013 0.013 0.013 0.015 Standard
    0.059 8-7628 42% 4.26 4.20 4.20 4.15 0.013 0.013 0.013 0.015 Standard

    Press Condition

    1. Heating rate(Rise of Rate) of material [Material Temperature]
    Programmable Press: 1.5-3.0℃/min (3~5℉/min).  Manual Press:3~6℃ /min (5~10℉/min)

    2. Curing Temperature & Time: >50min at more than 170℃ (338℉)[Material Temperature]

    3. Full Pressure : ≥250-280psi

    4. Vacuuming should be continued until over 140℃ (284℉) [Material Temperature]  

    5. Cold Press condition:  
    Keep Plate @ Room Temperature by water, Pressure:100psi, Keep Time:60minutes

    hot-start-cycle-vt-42s-manual.PNG adara-cedal-press-cycle-vt-42s.PNG hot-start-cycle-vt-42s.PNG

    Typical Drilling Parameters (φ0.3-1.0 mm)

    Desmearing Process

    Standard FR4 Desmear Process.
    Download PGL Datasheet